Research on the Preparation of Corrugated Board Paper by Blended Papermaking with Chemi-thermomechanical Pulping of Pre-hydrolyzed Corn Straw Substrate
Received:March 31, 2025  Revised:June 24, 2025
DOI:10.11980/j.issn.0254-508X.2025.11.015
Key Words:corn straw  pre-hydrolyzed chemi-thermomechanical pulping  OCC pulp  corrugated paper
Fund Project:宜宾市竹产业重大攻关项目(YBZD202401)。
Author NameAffiliationPostcode
HU Sisi* College of Materials Engineering, Fujian Agriculture and Forestry University, Fuzhou, Fujian Province, 350108) (*E-mail: hll65212@163.com 350108
CHENG Xinlei College of Materials Engineering, Fujian Agriculture and Forestry University, Fuzhou, Fujian Province, 350108) (*E-mail: hll65212@163.com 350108
LIN Danni College of Materials Engineering, Fujian Agriculture and Forestry University, Fuzhou, Fujian Province, 350108) (*E-mail: hll65212@163.com 350108
MIAO Qingxian College of Materials Engineering, Fujian Agriculture and Forestry University, Fuzhou, Fujian Province, 350108) (*E-mail: hll65212@163.com 350108
HUANG Fang College of Materials Engineering, Fujian Agriculture and Forestry University, Fuzhou, Fujian Province, 350108) (*E-mail: hll65212@163.com 350108
HUANG Liulian* College of Materials Engineering, Fujian Agriculture and Forestry University, Fuzhou, Fujian Province, 350108) (*E-mail: hll65212@163.com 350108
Hits: 2208
Download times: 748
Abstract:This study used pre-hydrolyzed corn stover-based chemi-thermomechanical pulp (C-CTMP) and old corrugated container (OCC) pulp as raw materials, aiming to enhance the properties of corrugated paper by optimizing refining, blending, and sizing processes. The results showed that after C-CTMP was refined with 5 000 r in a PFI mill (reaching a freeness of 45 °SR), the paper achieved optimal mechanical properties, including a breaking length of 5.64 km, burst index of 2.60 kPa·m²/g, tear index of 5.40 mN·m²/g, and ring crush index of 8.74 N·m/g. When C-CTMP mass ratio was 40%, the produced corrugated paper exhibited a density of 0.62 g/cm³, breaking length of 4.25 km, and ring crush index of 8.24 N·m/g, all demonstrating favorable mechanical performance. Furthermore, with the addition of 0.25% alkyl ketene dimer (AKD) and 1% dry cationic starch (both based on oven-dry pulp mass), the corrugated paper achieved a density of 0.60 g/cm³, breaking length of 4.56 km, ring crush index of 8.62 N·m/g, and water absorption Cobb60 value of 13.00 g/m², meeting the requirements for Grade AAA premium products under GB/T 13023—2008.