| Author Name | Affiliation | Postcode | | LYU Xiaofeng* | Zhejiang Jingxing Paper Industry Co., Ltd., Pinghu, Zhejiang Province, 314214 | 314214 | | NI Jianping | China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102 National Engineering Lab for Pulp and Paper Industry, Beijing, 100102 | 100102 | | FAN Shujie | China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102 National Engineering Lab for Pulp and Paper Industry, Beijing, 100102 | 100102 | | CHENG Zhengbai | Zhejiang Jingxing Paper Industry Co., Ltd., Pinghu, Zhejiang Province, 314214 | 314214 | | SUN Yanping | Zhejiang Jingxing Paper Industry Co., Ltd., Pinghu, Zhejiang Province, 314214 | 314214 | | LU Bin | Zhejiang Jingxing Paper Industry Co., Ltd., Pinghu, Zhejiang Province, 314214 | 314214 | | ZHOU Pingyan | Zhejiang Jingxing Paper Industry Co., Ltd., Pinghu, Zhejiang Province, 314214 | 314214 | | SU Zhenhua* | China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102 National Engineering Lab for Pulp and Paper Industry, Beijing, 100102 | 100102 |
|
| Hits: 2806 |
| Download times: 890 |
| Abstract:Within the recommended range, the moisturizing-locking performance of lab-grade moisturizing tissue increased with beating degree, reaching a peak value of 83.8% at a low-load beating level of 35 °SR. Since beating degree offered limited gains in wet strength, PAE 2 was introduced (20 kg/t pulp), significantly improving the wet tensile index and wet/dry ratio to 5.44 N·m/g and 13.6%, respectively. Wanfang cream (25% addition ) demonstrated excellent moisture-locking performance, achieving to 80.8%. Based on lab results, production trials were conducted with optimized beating processes: The long-fiber disc refiner configuration was adjusted from a single unit at 75 kWh/t to two 40 kWh/t units in series, the homogenizing refiner power was controlled at 18 kWh/t, and pulp flow rates and recirculation were adjusted. Trial-produced moisturizing base tissue showed significant improvements in bulk, dry tensile index (MD/CD), softness, and transverse liquid absorption height, approaching or reaching benchmark levels. The corresponding moisturizing tissue exhibited substantially enhanced moisturizing-locking performance: Trial—produced moisturizing tissue (trial—1, trial—2) achieved 1 h moisturizing-locking performance of 68.1% and 70.8% (baseline of 46.0%; benchmark of 52.7%), 2 h moisturizing-locking performance of 65.8% and 67.5% (baseline of 42.2%; benchmark of 50.0%), and 3 h moisturizing-locking performance of 60.1% and 63.3% (baseline of 35.7%; benchmark of 46.6%), far exceeding both the baseline and benchmark. |
| View Full Text HTML View/Add Comment Download reader |
|
|
|