本文二维码信息
二维码(扫一下试试看!)
Study on Oil Resistance of Different Kinds of Grinding Starch Used in Paper Food Packaging
Received:September 14, 2024  
DOI:10.11980/j.issn.0254-508X.2025.01.008
Key Words:food packaging  grinding starch  oil resistance level  oil absorption value  oil contact angle
Author NameAffiliationPostcode
ZHANG Ruijuan China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102
National Engineering Lab for Pulp and Paper, Beijing, 100102 
100102
SU Yanqun China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102
National Engineering Lab for Pulp and Paper, Beijing, 100102 
100102
XIA Fei China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102
National Engineering Lab for Pulp and Paper, Beijing, 100102 
100102
LIU Jingang* China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102
National Engineering Lab for Pulp and Paper, Beijing, 100102 
100102
XIAO Guihua China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102
National Engineering Lab for Pulp and Paper, Beijing, 100102
School of Light Industry and Engineering, South China University of Technology, Guangzhou, Guangdong Province, 510640 
510640
SUN Dewen China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102
National Engineering Lab for Pulp and Paper, Beijing, 100102 
100102
YANG Xiaobo China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102
National Engineering Lab for Pulp and Paper, Beijing, 100102 
100102
HUANG Ju China National Pulp and Paper Research Institute Co., Ltd., Beijing, 100102 100102
Hits: 3033
Download times: 1110
Abstract:Ultrafine grinding starch dispersion was prepared by mechanical progress and coated on the surface of white cardboard for food packaging. Then the effect of starch type, size of grinding starch and coating amount on oil resistance of white cardboard was studied. The results showed that grinding cationic starch and grinding highly crosslinked starch M were more beneficial to improve the oil resistance of white cardboard. In addition, the smaller the grinding starch particles size and the higher the coating amount, the higher the oil resistance level of white cardboard. Using highly crosslinked starch M as raw material with size of 0.264 μm, and the coating amount of 3.5 g/m2, the air permeability of coated white paperboard was reduced by 98.0%, the oil resistance level reached to 6, the oil absorption value reached to 0.87g/m2, and the oil contact angle reached to 93.2°. When the coating amount increased from 2.23 g/m2 to 6.20 g/m2, the oil resistance level of coated white paperboard increased from 2 to 9, and the air permeability decreased from 0.059 3 to 0.000 081 0 μm·Pa·s, the oil absorption decreased from 2.32 g/m2 to 0.59 g/m2.
View Full Text  HTML  View/Add Comment  Download reader