Study on Preparation and Strength Properties of Corrugated Medium Using Bamboo Pulp and Camphor Residue Pulp
Received:September 25, 2023  
DOI:10.11980/j.issn.0254-508X.2024.04.007
Key Words:natural bamboo pulp  sieve  camphor residue  paper making  corrugated medium
Fund Project:2022年宜宾市科技局“揭榜挂帅”项目;宜宾市科技计划项目(2022JB010,2022JB009,2022JC001);教育部产学合作协同育人项目(202102072055);四川轻化工大学2023年大学生创新创业训练计划项目(CX2023131)。
Author NameAffiliationPostcode
JIANG Feng Sichuan University of Science & Engineering Zigong Sichuan Province 643000 643000
TANG Min Sichuan Yibin Forest and Bamboo Industry Research Institute Yibin Sichuan Province 644000 644000
ZHAO Ju Sichuan Papermaking Product Quality Supervision and Inspection Centre Leshan Sichuan Province 614000 614000
YANG Ling* Sichuan University of Science & Engineering Zigong Sichuan Province 643000 643000
LI Wenjun Sichuan University of Science & Engineering Zigong Sichuan Province 643000 643000
XU Mingxian Sichuan University of Science & Engineering Zigong Sichuan Province 643000 643000
ZHANG Shengquan Sichuan University of Science & Engineering Zigong Sichuan Province 643000 643000
LIU Xinhai Sichuan University of Science & Engineering Zigong Sichuan Province 643000 643000
ZHAO Xingtao Sichuan University of Science & Engineering Zigong Sichuan Province 643000 643000
Hits: 740
Download times: 4
Abstract:In this study, the commercially available natural bamboo pulp was sieved, the short-fibre bamboo pulp with partide size<0.6 mm and oil evaporation of camphor residue pulp were selected to prepare corrugated medium. The results showed that when 25% soft wood pulp, 0.5% cationic starch (CS), 0.4% cationic polyacrylamide (CPAM) ,and 1.8% polyamide epichlorol resin (PAE, concentration of 9.5%) were added, short-fibre bamboo pulp (unbeaten) and camphor residue pulp were used to prepare paper with the mass ratio of 10∶90 without cure treatmeut, the paper splitting length was 2.66 km, the cyclic compression index was 5.60 N·m/g, which met the requirements for the qualified products of GB/T 13023—2008.When the short-fibre bamboo pulp was beat to a degree of 35.8 °SR, and the camphor residue pulp was added with the mass ratio of 30∶70, after cure treatment 110 ℃ for 15 min, the paper was obtained with splitting length of 4.75 km, cyclic compression index of 8.24 N·m/g,breakage resistance index of 2.80 kPa·m2/g, folding resistance of 15, of which the splitting length and the cyclic compression index reached the requirements for the superior grade of GB/T 13023—2008 , breakage resistance index and folding resistance indicators were up to the requirements for qualified products of GB/T 13024—2016.