二维码(扫一下试试看!) |
Study on Preparation and Strength Properties of Corrugated Medium Using Bamboo Pulp and Camphor Residue Pulp |
Received:September 25, 2023 |
DOI:10.11980/j.issn.0254-508X.2024.04.007 |
Key Words:natural bamboo pulp sieve camphor residue paper making corrugated medium |
Fund Project:2022年宜宾市科技局“揭榜挂帅”项目;宜宾市科技计划项目(2022JB010,2022JB009,2022JC001);教育部产学合作协同育人项目(202102072055);四川轻化工大学2023年大学生创新创业训练计划项目(CX2023131)。 |
|
Hits: 953 |
Download times: 4 |
Abstract:In this study, the commercially available natural bamboo pulp was sieved, the short-fibre bamboo pulp with partide size<0.6 mm and oil evaporation of camphor residue pulp were selected to prepare corrugated medium. The results showed that when 25% soft wood pulp, 0.5% cationic starch (CS), 0.4% cationic polyacrylamide (CPAM) ,and 1.8% polyamide epichlorol resin (PAE, concentration of 9.5%) were added, short-fibre bamboo pulp (unbeaten) and camphor residue pulp were used to prepare paper with the mass ratio of 10∶90 without cure treatmeut, the paper splitting length was 2.66 km, the cyclic compression index was 5.60 N·m/g, which met the requirements for the qualified products of GB/T 13023—2008.When the short-fibre bamboo pulp was beat to a degree of 35.8 °SR, and the camphor residue pulp was added with the mass ratio of 30∶70, after cure treatment 110 ℃ for 15 min, the paper was obtained with splitting length of 4.75 km, cyclic compression index of 8.24 N·m/g,breakage resistance index of 2.80 kPa·m2/g, folding resistance of 15, of which the splitting length and the cyclic compression index reached the requirements for the superior grade of GB/T 13023—2008 , breakage resistance index and folding resistance indicators were up to the requirements for qualified products of GB/T 13024—2016. |
View Full Text HTML View/Add Comment Download reader |