 二维码(扫一下试试看!) |
| Coating Solution to Decrease Energy Consumption and Paper Dust of Tissue Paper |
| Received:April 10, 2021 |
| DOI:10.11980/j.issn.0254-508X.2021.09.018 |
| Key Words:tissue adhesive release low-temperature coating paper dust steam |
| Author Name | Affiliation | E-mail | | WANG Bo* | Vinda International Holdings Ltd., Jiangmen, Guangdong Province, 529100 | wb@vinda. com | | LIAO Chang | Vinda Paper (China) Co., Ltd., Jiangmen,Guangdong Province,529100 | | | YANG Zhifu | Vinda Paper (Zhejiang) Co., Ltd.,Quzhou, Zhejiang Province,324400 | | | ZHAO Zhisong | Jining Nantian Nongke Chemical Co., Ltd., Jining, Shangdong Province,372200 | | | LI Taowei | Jining Nantian Nongke Chemical Co., Ltd., Jining, Shangdong Province,372200 | | | HUANG Jun | Jining Nantian Nongke Chemical Co., Ltd., Jining, Shangdong Province,372200 | | | MA Pu | Jining Nantian Nongke Chemical Co., Ltd., Jining, Shangdong Province,372200 | | | MA Yuqin | Jining Nantian Nongke Chemical Co., Ltd., Jining, Shangdong Province,372200 | | | ZHANG Weiping | Jining Nantian Nongke Chemical Co., Ltd., Jining, Shangdong Province,372200 | |
|
| Hits: 6452 |
| Download times: 3867 |
| Abstract:The clean production of tissue included paper dust control and energy consumption control. In order to reduce paper dust and steam consumption, low-temperature coating products were targeted developed to replace conventional coating products. The characteristics of low-temperature adhesive, low-temperature release and low-temperature coating were studied in this paper. The results showed that the low-temperature adhesive had high adhesion, suitable water resistance and suitable film forming hardness at lower temperature. The low-temperature release had lower surface tension and suitable peel force, and the nano scale low-temperature release could be distributed more evenly in the coating. The stability of the mixture of low-temperature adhesive and low-temperature release was tested by Turbiscan stability instrument. The TSI coefficient was only 0.98, indicating that the mixture was stable. After industrial application of low-temperature coating, it was found that under the same conditions, the steam pressure of Yankee cylinder could be reduced by 80~230 kPa, and the steam consumption could be reduced to a certain extent. Compared with conventional coating, the application of low-temperature coating could reduce the dust drop rate of base paper/finished products by 10%~50%. |
| View Full Text HTML View/Add Comment Download reader |
|
|
|