 二维码(扫一下试试看!) |
| Study on the Treatment of Tobacco Sheet by Fe-CA Biomimetic System |
| |
| DOI:10.11980/j.issn.0254-508X.2011.05.006 |
| Key Words:tobacco sheet biomimetic lignin tensile strength softness degree smoking |
| Fund Project:本课题为国家自然科学基金(31070521,30871996)资助项目。 |
| Author Name | Affiliation | | 刘志昌1 | 1.湖北中烟技术中心重组烟叶应用技术研究湖北省重点实验室,湖北武汉,430040 | | 王学文1 | 1.湖北中烟技术中心重组烟叶应用技术研究湖北省重点实验室,湖北武汉,430040 | | 唐向兵1 | 1.湖北中烟技术中心重组烟叶应用技术研究湖北省重点实验室,湖北武汉,430040 | | 安 瑞2 | 2.湖北工业大学化学与环境工程学院,湖北武汉,430068 | | 王 磊2 | 2.湖北工业大学化学与环境工程学院,湖北武汉,430068 | | 谢益民2 | 2.湖北工业大学化学与环境工程学院,湖北武汉,430068 |
|
| Hits: 9486 |
| Download times: 2464 |
| Abstract:The tobacco(stem,scrap) treated by Fe-CA biomimetic system was used to made tobacco sheet by using a sheet former, through the orthogonality experiment the optimum treatment conditions of the tobacco(stem,scrap) are achieved as following: reaction temperature 45℃; reaction time 30 minutes; dosage of biomimetic 20mmol/kg tobacco; H2O2 1%. The tensile strength and softness of the tobacco sheet produced under the optimum condition increased about 5.19% and 11.43% respectively compared with the control sample. At the same time, smoking assessment indicates that the aroma, bad odor and harmony of the tobacco improve in certain degree, woody odor reduces, the stimulation of tobacco reduces and quality is improved. |
| View Full Text HTML View/Add Comment Download reader |
|
|
|