Application of Wollastonate in Surface Sizing of Corrugating Medium
  
DOI:10.11980/j.issn.0254-508X.2014.05.007
Key Words:wollastonite  starch  surface sizing  ring crush strength
Author NameAffiliation
陈夫山 青岛科技大学化工学院山东青岛266042 
常建栋 青岛科技大学化工学院山东青岛266042 
宋晓明 青岛科技大学化工学院山东青岛266042 
宋鹏瑶 青岛科技大学化工学院山东青岛266042 
Hits: 5086
Download times: 1618
Abstract:The paper mainly studied the application of wollastonate in corrugating medium surface sizing. The surface sizing starch, wollastonite and starch replacement agent were gelatinized to use as the surface size. Experiments showed that when 10% of surface sizing starch was replaced with the wollastonite, the CD ring crush strength increased to 5.30 N·m/g, and MD ring crush index increased to 7.55 N·m/g; CD tensile index increased to 46.2 N·m/g, and MD tensile index increased to 95.9 N·m/g; CD folding strength increased to 11 times and MD folding strength increased to 35 times.
View Full Text  HTML  View/Add Comment  Download reader